Whether you print at home or order prints, it helps to recognise the common defects and know where they come from. Most have a handful of causes, and many can be fixed in the design rather than at the printer.

Warping: corners lifting off the bed

What you see: the bottom corners of a part curl up, leaving it rocking on a flat surface.

Why: plastic shrinks as it cools. On large flat parts, the top layers pull on the bottom ones until the corners lift. ABS shrinks the most, PLA the least.

Fixes:

  • Print warping-prone materials (ABS, ASA, nylon) in an enclosed printer that keeps the air warm.
  • Keep the build plate clean and use the right bed temperature and adhesive for the material.
  • In the design, round sharp corners on large flat parts. Corners are where lifting starts.
  • Avoid long, thin, flat parts in ABS where possible, or switch to PETG.

Stringing: fine hairs between features

What you see: thin strands of plastic stretched between separate parts of the print, like a cobweb.

Why: molten plastic oozes from the nozzle as it travels between features. PETG is especially prone to it, and damp filament makes it much worse.

Fixes:

  • Dry the filament. Most filaments absorb moisture from the air, and Indian monsoon humidity makes this a real problem. Damp filament strings, bubbles and prints weaker.
  • Tune retraction and print temperature.
  • Light strings come off in seconds with a heat gun or by brushing.

Layers splitting apart

What you see: cracks between layers, or a part that snaps cleanly along a layer line.

Why: layers did not fuse well. Causes include printing too cold, too much cooling fan on ABS, drafts, or simply a part loaded across its layers.

Fixes:

  • Raise the print temperature and reduce cooling for the material.
  • Use an enclosure for ABS and ASA.
  • Reorient the part so the load runs along the layers. This matters more than any setting. See designing parts for 3D printing.

Brittle parts that snap

What you see: a clip or hook that breaks the first time it flexes.

Why: usually the material. PLA and standard resin are stiff and brittle. Damp filament also prints weaker.

Fixes: use PETG for parts that bend or clip, keep filament dry and orient the part so it bends along its layers. Our material guide helps you choose.

Elephant's foot

What you see: the bottom few layers bulge outwards slightly, so a part will not fit flush into a slot.

Why: the first layer is pressed onto the bed for adhesion and spreads a little.

Fixes: add a small 0.3 to 0.5 mm chamfer to the bottom edge in your design, or adjust first-layer settings.

Holes and fits too tight

What you see: bolts do not pass through, and parts that should slide together do not.

Why: printed holes come out slightly small, and parts need clearance designed in.

Fixes: design in clearance (about 0.3 to 0.4 mm for sliding parts) and slightly enlarge holes, or drill them to size.

Visible layer lines and rough surfaces

Layer lines are normal on FDM prints. Finer layers reduce them at the cost of print time. For smooth surfaces, choose resin for small parts or ask for sanding and priming on FDM parts.

Let us handle it